EP40ND

Two component, room temperature curing epoxy with good toughness, paste consistency
Key Features
  • Convenient handling
  • Good bond strength in shear and peel modes
  • Exceptional adhesion to polycarbonates and acrylics
  • Meets NASA low outgassing
    Typical Properties
    Viscosity
    Part A: 50,000-100,000 cps, Part B: paste
    Cure Schedule
    overnight at 75°F, followed by a post cure at 120-150°F for 2-3 hours
    Hardness
    50-60 Shore D
    Service Temperature Range
    -100°F to +250°F
    Elongation
    80-90%
    Tensile Lap Shear Strength
    1,600-1,800 psi
    תמונה
    EP40ND Two Part Epoxy System
    Certifications

    ASTM E595 Compliant

    Meets EU Directive 2015/863

    Product Description

    Master Bond EP40ND is a two part, room temperature curing epoxy for bonding, sealing, and coating. This non-drip system has a forgiving 1:1 mix ratio by weight or volume. It is formulated to cure readily at ambient temperatures or more rapidly at elevated temperatures. The optimum curing schedule is overnight at room temperature followed by 2-3 hours at 120°F to 150°F. EP40ND is 100% reactive and contains no solvents or diluents.

    EP40ND is a superb adhesive and bonds well to a variety of substrates including metals, ceramics, composites and plastics. It is most noteworthy for its affinity to bonding engineered plastics such as polycarbonates and acrylics. EP40ND is also capable of withstanding rigorous thermal cycling and shock. EP40ND is a reliable electrical insulator. It is a relatively low exothermic system and can be applied in thick sections. It withstands many common chemicals including water, oils, fuels, cleaning agents and some acids and bases. The color of Part A is translucent and Part B is amber. The service temperature range is -100°F to +250°F. There are many applications in electronics, opto-electronics and medical devices that utilize plastic substrates, which may be prone to stress cracking. It is important to select an adhesive that mitigates this possibility. EP40ND is an excellent candidate for these types of applications.

    Product Advantages

    • Convenient handling, 1:1 mix ratio
    • Long open time
    • Paste consistency
    • Good lap shear and outstanding peel strength
    • High elongation
    • Highly compatible with bonding polycarbonates and acrylics
    Show More

    How to order

    Verify Your Product Selection

    With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

    Get a Quote

    Our customer service team will follow up with a detailed quote with packaging and shipping options.

    Place Your Order

    We'll work with your company to process the order efficiently.

    Receive Your Material

    Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.