EP42HT-2ND-2Med Black
Two component, high temperature resistant epoxy compound for medical device assembly
Key Features
- Paste consistency
- Convenient processing
- Meets USP Class VI and ISO 10993-5
- Resists repeated sterilization
Typical Properties
Viscosity
Part A: >1,000,000 cps, Part B: >250,000 cps
Cure Schedule
overnight at 75°F followed by 6-8 hours at 135-165°F or 4-6 hours at 175-185°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.0
Glass Transition Temperature (Tg)
150-155°C