EP42HT-3AO

Two part, room temperature curable epoxy adhesive, sealant, coating and encapsulating system
Key Features
  • Convenient handling, long working life
  • Thermal conductive and electrical insulative
  • High glass transition temperature
  • Low coefficient of thermal expansion
Typical Properties
Viscosity
40,000-80,000 cps
Cure Schedule
Cure in 3-4 days at 75°F or 2-3 hours at 150-200°F; Recommended curing is overnight at 75°F followed by 2-3 hours at 150-200°F; Optimum cure schedule: Overnight at 75°F, followed by 2-3 hours at 150-200°F
Hardness
85-95 Shore D
Service Temperature Range
4K to +400°F
Acoustical Impedance
5.3 MRayl
Glass Transition Temperature (Tg)
140-150°C
תמונה
EP42HT-3AO Two Part Epoxy
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Packaging
Product Description

Master Bond EP42HT-3AO is thermally conductive, electrically insulating epoxy for bonding, sealing, coating and encapsulation applications. It is relatively easy to use with a forgiving 100 to 40 mix ratio by weight. It will cure in 3-4 days at room temperature or 2-3 hours at 150-200°F. To optimize properties, the recommended curing is overnight at room temperature followed by 2-3 hours at 150-200°F. Upon mixing, EP42HT-3AO is a moderate viscosity system with very good flow properties.

Among its many favorable attributes, this system has a high glass transition temperature and a low coefficient of thermal expansion. It bonds well to a wide variety of substrates including metals, composites, ceramics, glass and many plastics. Some positives include its low shrinkage upon curing and stellar dimensional stability. It is resistant to water, oils, acid, bases and many solvents. The service temperature range is from 4K to +400°F. The color of Part A is white and the color of Part B is off-white. This blend of product properties allows this distinctive formulation to be used in specialty electronic, optical, opto-electronic, aerospace and related industries.

Product Advantages

  • Forgiving 100:40 mix ratio by weight
  • Good flow, long working life
  • Superior thermal and dimensional stability
  • Cryogenically serviceable
  • Combines low CTE and high Tg
  • Meets NASA low outgassing specification
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.