EP45HTAN
Two component, high strength epoxy system
Key Features
- Easy to work with
- Thermally conductive and electrically insulative
- Superior dimensional stability
- Excellent strength retention at high temperatures
- Cryogenically serviceable
- Bonds well to metals, especially roughened titanium
Typical Properties
Viscosity
thixotropic paste
Cure Schedule
2-3 hours at 300°F followed by a post cure of 3-4 hours at 350°F
Hardness
80-90 Shore D
Service Temperature Range
4K to +500°F
Dielectric Constant
4.6
Tensile Lap Shear Strength
2,300-2,500 psi
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
Case Study
EP45HTAN: Used for bonding titanium to carbon-carbon composites for use under extreme temperatures
Can an adhesive maintain its strength when bonding titanium to carbon-carbon composites under extreme temperature and harsh conditions? This is precisely what researchers1 from QSS Group, Inc., the Ohio Aerospace Institute and the NASA Glenn Research …