EP4UF-80

One component epoxy for bonding and underfill applications, minimum curing temperature 80°C
Key Features
  • Thermally conductive and electrically insulating
  • Ultra fine particle size
  • Low viscosity and good flow
  • NASA low outgassing
Typical Properties
Viscosity
500-1,500 cps
Cure Schedule
30-60 minutes at 80-85°C, or 15-30 minutes at 90-95°C
Hardness
85-95 Shore D
Service Temperature Range
-58°F to +302°F
Glass Transition Temperature (Tg)
150-155°C
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP4UF-80 One Component Epoxy
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Packaging
Product Description

Master Bond EP4UF-80 is a one component, low viscosity epoxy primarily for underfill applications, that can also be used as an adhesive. It has good flow properties and will cure at elevated temperatures with a minimum of 80°C. It is shipped at -40°C and should be stored at that temperature. Once removed from the freezer, for optimum results, use the epoxy within 6 hours. Any remaining material should be discarded. Curing is simple and straightforward; 30-60 minutes at 80-85°C, or 15-30 minutes at 90-95°C. EP4UF-80 has a thermally conductive, electrically insulative filler material with ultra small particle sizes. This allows EP4UF-80 to be used as an underfill in spaces as small as 10-15 microns wide. As an underfill system, EP4UF-80 has high mechanical strength properties, outstanding dimensional stability and low shrinkage upon curing.

EP4UF-80 is a highly useful thermally conductive adhesive. It bonds well to a variety of substrates such as metals, composites, ceramics and many plastics. Because the particles are so small, it can be applied in thin bond sections. This, in effect, lowers the thermal resistance and increases the heat transfer properties of the system. For example, with a typical thermally conductive filler, a reasonable bond line thickness is about 50 microns. In this scenario, the thermal resistance would be 50-100 x 10-6 K•m2/W. However, when an epoxy such as EP4UF-80 is applied, the thin bond line lowers the thermal resistance to 10-20 x 10-6 K•m2/W. This is a big positive in managing heat related issues. EP4UF-80 will resist waters, oils and fuels. Its color is gray. The service temperature range is -50°C to +150°C. The system is a highly effective thermal interface material for bonding and underfill applications in microelectronic packaging and assembly.

Product Advantages

  • Single component; no mixing needed
  • Rapid curing with versatile cure schedules
  • Can be used as an underfill for very tight spaces
  • Small particle size lowers thermal resistance
  • High modulus
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.