EP51FL-1

Two component room temperature curing epoxy system for bonding, sealing and coating
Key Features
  • Exceptional flexibility
  • Superb electrical insulation properties
  • Very rapid curing
  • Higher viscosity
Typical Properties
Viscosity
Part A: 10,000-14,000 cps, Part B: 130,000-160,000 cps
Cure Schedule
30-40 minutes at 75°F and full cure within 24 hours at 75°F; another alternative cure schedule is 2-3 hours at 75°F followed by an hour at 150-200°F
Hardness
10-20 Shore D
Service Temperature Range
-100°F to +250°F
Elongation
>200%
Volume Resistivity
>10¹⁵ ohm-cm
תמונה
EP51FL-1 Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP51FL-1 is a two component, highly flexible epoxy resin system for high performance bonding, sealing and coating featuring a very rapid set up time and cure. Most flexiblilized epoxy formulations are slower curing, but EP51FL-1 cures much more quickly. It typically has a set up time of 30-40 minutes and full cure within 24 hours at room temperature. Another alternative cure schedule is 2-3 hours at room temperature followed by an hour at 150-200°F. It has a one to three mix ratio by weight or by volume. Some of the outstanding properties of this system are exceptionally high peel strength and elongation. Its excellent flexibility allows it to be used in applications involving thermal cycling, harsh thermal and mechanical shocks and other situations where superior toughness is desirable. EP51FL-1 bonds well to many different substrates including metals, plastics and many types of rubber. In fact, it may adhere well to untreated rubber materials such as neoprene, nitrile, SBR and occasionally EPDM rubber compounds; materials that normally require time consuming surface preparation. It has very good chemical resistance to oils, fuels and water. EP51FL-1 is a first class electrical insulator. Its service temperature range is -100°F to +250°F with superior low temperature serviceabilty. EP51FL-1 is widely used in the aerospace, electronic, electrical, repair and maintenance and specialty OEM industries where good flexibility and fast cure are desirable property traits.

Product Advantages

  • Non-critical one to three mix ratio by weight or volume
  • Easy application; higher viscosity epoxy spreads evenly and smoothly
  • Very fast set up time and cure
  • High peel strength and elongation
  • Readily withstands rigorous thermal cycling and severe thermal and mechanical shock resistance
  • Superior adhesion to a wide variety of substrates
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.