EP62-1LPSPMed White

Two component, high performance epoxy system featuring biocompatibility for bonding, sealing, coating, encapsulating and impregnation
Key Features
  • Convenient handling
  • Pigmented white
  • Capable of resisting repeated sterilization
  • Passes ISO 10993-5 requirements
Typical Properties
Viscosity
150-300 cps
Cure Schedule
Overnight at 75°F followed by either 8-10 hours at 60-70°C, 60-90 minutes at 80-100°C, or 30-60 minutes at 125°C. Post curing at 110-135°C for 2-4 hours will help optimize properties.
Hardness
75-85 Shore D
Service Temperature Range
4K to +400°F
Dielectric Constant
4.6
Glass Transition Temperature (Tg)
80-85°C
תמונה
Two Part Epoxy EP62-1LPSPMed White
Product Description

Master Bond EP62-1LPSPMed White is a two part, very low viscosity epoxy that passes ISO 10993-5 certifications. It has a forgiving mix ratio of 100 to 25 by weight. Upon mixing, the viscosity is markedly low and the working life is lengthy, 12-24 hours at room temperature. The recommended cure schedule is overnight at room temperature followed by either 8-10 hours at 60-70°C, 60-90 minutes at 80-100°C, or 30-60 minutes at 125°C. To obtain optimal properties, use one of the schedules above, followed by a post cure of 110-135°C for 2-4 hours. This epoxy contains no solvents or diluents and has low shrinkage upon curing..

The system bonds well to a wide variety of substrates including metals, composites, glass, rubber and many plastics. It has an attractive array of physical strength properties and is a reliable electrical insulator. EP62-1LPSPMed White offers superior resistance to EtO, radiation, chemical sterilization and autoclaving. It can be used for both reusable and disposable medical devices. Its low viscosity makes it viable for small potting and encapsulating applications. The system has a degree of toughness that allows for thermal cycling, and the ability to withstand mechanical shock and vibration. Its temperature range extends from 4K to +400°F. This compound is an attractive candidate for medical devices where a low viscosity, white colored, sterilization resistant epoxy is desirable.

Product Advantages

  • Forgiving 100 to 25 mix ratio by weight
  • Ultra low viscosity
  • Long working life
  • Withstands chemical sterilants and autoclaving
  • Wide temperature range
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.