Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 8,000-12,000 cps
Cure Schedule
3-5 minutes setup, full cure within 6-12 hours at 75°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +400°F
Dielectric Constant
4.1
Glass Transition Temperature (Tg)
125-130°C
תמונה
EP65HT-1 Two Part Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

וידאו

How to Apply Super Fast Curing Epoxy

In this demonstration, Master Bond EP65HT-1 epoxy is used to show how a fast curing compound can set up quickly at room temperature. This two part system is commonly utilized for advanced engineering applications. It is a sure winner to speed up your …
Product Description

Master Bond EP65HT-1 is a specialty type system that features the unusual combination of ultra fast curing and high temperature resistance. While typical fast setting epoxies normally possess glass transition temperatures (Tg) below 85°C, EP65HT-1 has an exceptional Tg of approximately 125°C. In addition, unlike typical fast cure epoxies, EP65HT-1 retains fast setup times even when mixed in relatively small masses. EP65HT-1 normally will setup in 3-5 minutes in 10-20 gram masses. A full cure generally occurs within 6-12 hours with high tensile shear strengths of over 1,200 psi. This system offers good physical properties, including low shrinkage upon cure, excellent dimensional stability and a high tensile modulus. The service temperature range is -60°F to +400°F. EP65HT-1 offers sound electrical insulating properties and a useful chemical resistance profile. EP65HT-1 fully meets the NASA low outgassing specifications and is particularly well suited for vacuum applications.

EP65HT-1 bonds well to a wide variety of substrates including metals, glass, ceramics, vulcanized rubbers and many plastics. Dispensing EP65HT-1 can be greatly facilitated by utilizing a dispensing gun capable of mixing fast setting materials with a ten to one mix ratio. This system is 100% reactive and does not contain any solvents. Part A is clear, and Part B is dark brown in color. It is especially useful for both prototyping and manufacturing in the aerospace, electronic, optical, electro-optical, vacuum related as well as specialty OEM applications where the special blend of fast curing and high temperature resistance is desirable.

Product Advantages

  • Ultra fast setting and curing even in small masses; very short fixturing time
  • Exceptionally high heat resistance
  • Good physical strength properties
  • Superior electrical insulation properties
  • Available with convenient dispensing gun
  • NASA low outgassing certified
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.