LED405FL3
One component, flexibilized LED curable system
Key Features
- Fast cure with appropriate LED light
- Not oxygen inhibited
- Outstanding optical clarity, with fluorescent dye
- Can cure up to 1/8 inch thick
Typical Properties
Viscosity
500-3,000 cps
Cure Schedule
Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections.
Hardness
5-15 Shore D
Service Temperature Range
-100°F to 250°F
Refractive Index
1.51
Volume Resistivity
>10¹⁴ ohm-cm