LED405Med

One component, nanosilica filled LED curable system
Key Features
  • Meets ISO 10993-5 for cytotoxicity
  • Fast cure with appropriate LED light
  • Resists sterilization
  • Not oxygen inhibited
  • Can cure up to 1/8 inch thick
  • Outstanding optical clarity
Typical Properties
Viscosity
2,000-8,000 cps
Cure Schedule
Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections.
Hardness
65-75 Shore D
Service Temperature Range
-60°F to +250°F
Coefficient of Thermal Expansion
35-40 X 10⁻⁶ in/in/°C
Dielectric Constant
4.2
תמונה
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Product Description

Master Bond LED405Med is a one part system that cures upon exposure to a 405 nm LED light without requiring a UV light source. It will cure without any oxygen inhibition. Its most special feature is that its main constituent is a nanofilled resin. This results in lower shrinkage upon curing and greater dimensional stability. By using LED light and not UV, it is intrinsically less hazardous and more user friendly.

Master Bond LED405Med requires no mixing and cures rapidly upon exposure to 405 nm LED light. The speed of cure depends upon the intensity of the light source, the thickness of the layer, and the distance of the light source from the material being cured. Realistically, the light intensity should be 1-4 watts/cm2. Master Bond strongly advises end users to consult with their LED light provider in order to choose the best light source.

LED405Med will typically cure in 30-45 seconds in thinner sections, while thicker sections will take longer to cure. LED405Med bonds well to a wide variety of substrates including metals, plastics and glass. It is a superior electrical insulator and is resistant to water, several acids and bases, as well as oils and fuels. LED405Med resists many sterilization methods such as gamma, EtO and radiation. It has a particular affinity for acrylics, polycarbonates, and glass.

Product Advantages

  • One component system needs no mixing
  • Cures by LED light, UV light not required
  • Nanofilled system
  • Unsurpassed low shrinkage upon curing
  • Reasonably good physical strength properties
  • Superb dimensional stability
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.