LED415DC90

One component, flexibilized LED curable system
Key Features
  • Cures rapidly with LED light
  • Secondary heat cure at 90-95°C
  • Can cure up to 6 mm deep or in cross section
  • Formulated for “side bonding” applications
Typical Properties
Viscosity
25,000-250,000 cps
Cure Schedule
Cures rapidly upon exposure to LED light at 405 nm followed by heat curing at 90-95°C for 30-45 minutes
Hardness
85-90 Shore D
Service Temperature Range
-80°F to +350°F
Tensile Modulus
450,000-550,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
One Part Adhesive LED415DC90
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond LED415DC90 is a one part system that cures rapidly upon exposure to LED light at 405 nm followed by heat curing at 90-95°C for 30-45 minutes. This fast curing system is not oxygen inhibited and can cure up to 6 mm deep or in cross section. This unusual curing profile allows this LED to be used for side bonding. Side bonding refers to a situation where the LED is applied between two opaque substrates and the light is exposed to the adhesive from a side angle and not through the substrate, which is more the norm. The unusually deep penetration in cross section offered by LED415DC90 allows it to partially cure enough to fixture the two substrates. The cure is then completed by adding 90-95°C heat for 30-45 minutes.

There are some variables to consider with speed of the LED curing process. These include the intensity of the light source, the thickness of the layer, and the width of the cross section that is being cured. The recommended intensity of the light source should be 2-4 watts/cm2.

LED415DC90 bonds well to a wide variety of substrates including plastics, glass and metals. The system has good chemical resistance to oil, water, fuels, and mild acids and bases. It is a reliable electrical insulator with a service temperature range of -80°F to 350°F. Additionally, it can withstand rigorous thermal cycling, mechanical shock and vibration. The special feature of LED415DC90 curing well cross sectionally combined with its secondary heat cure allows it to be used as a high strength adhesive. Utilizing LED light for fixturing followed by relatively fast heat curing is an interesting and unique way of attaching substrates together.

Product Advantages

  • One component system
  • Cures by LED light, UV light not required
  • Uncured material readily polymerizes with heat
  • Can cure in cross section 4-6 mm
  • Excellent strength properties, especially lap shear
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.