LED415DC90Med

One component, dual curing LED/heat system that allows for rapid LED initiated fixturing followed by full cure by adding heat; meets ISO 10993-5
Key Features
  • Rapid cure initiation with LED light
  • Cure completed at 90-95°C
  • Formulated for side bonding applications
  • Can cure up to 6 mm deep or in cross section
Typical Properties
Viscosity
25,000-250,000 cps
Cure Schedule
cures rapidly upon exposure to LED light at 405 nm followed by heat curing at 90-95°C for 30-45 minutes
Hardness
85-90 Shore D
Service Temperature Range
-80°F to +350°F
Dielectric Constant
4.5
Tensile Modulus
450,000-550,000 psi
תמונה
LED415DC90Med One Part LED and Heat Curing Adhesive
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Product Description

Master Bond LED415DC90Med is a one part system that cures rapidly upon exposure to LED light at 405 nm followed by heat curing at 90-95°C for 30-45 minutes. This fast curing system is not oxygen inhibited and can cure up to 6 mm deep or in cross section. This unusual curing profile allows the system to be used for side bonding. Side bonding refers to a situation where the LED is applied between two opaque substrates and the light is exposed to the adhesive from a side angle and not through the substrate, which is more typical. The unusually deep penetration in cross section offered by LED415DC90Med allows it to partially cure enough to fixture the two substrates.

The recommended intensity of the light source should be 2-4 watts/cm2, but there are some variables to consider with speed of the LED curing process. These include the intensity of the light source, the thickness of the layer, and the width of the cross section that is being cured.

LED415DC90Med bonds well to a wide variety of substrates including plastics, glass and metals. The system has good resistance to medical sterilants such as gluteraldehyde, peracetic acid, as well as EtO, gamma radiation, among others. It is a reliable electrical insulator with a service temperature range of -80°F to 350°F. Additionally, it can withstand rigorous thermal cycling, mechanical shock and vibration. The main attraction of this one part system is its rapid cure that utilizes LED light for the initiation of polymerization, followed by completion of curing by heating. The combination of fast, easy processing and good physical strength properties, along with ISO 10993-5 compliance, opens creative new horizons for using adhesives in medical device manufacturing.

Product Advantages

  • One component system
  • Fast dual curing system, LED light and heat
  • Excellent strength properties, especially lap shear
  • Can cure in cross sections 4-6 mm
  • Meets ISO 10993-5
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.