LED422DC90

One component, nanosilica filled dual curing LED system allowing for rapid fixturing and subsequent curing by heat. Complies with NASA low outgassing
Key Features
  • Fixtures rapidly with LED light
  • Secondary heat cure at 90-95°C
  • Can cure 2-3 mm deep or in cross section
  • Formulated for “side bonding” applications
Typical Properties
Viscosity
2,000-15,000 cps
Cure Schedule
exposure to LED light at 405 nm which induces polymerization in a cross sectional mode, 2-3 mm deep. The cure is then completed by adding heat at 90-95°C for 30-45 minutes.
Hardness
85-90 Shore D
Service Temperature Range
-80°F to +350°F
Refractive Index
1.49
Tensile Modulus
475,000-575,000 psi
תמונה
LED422DC90 One Part LED and Heat Curing Adhesive
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Product Description

Master Bond LED422DC90 is a one part, nanosilica based system that cures rapidly in a two tiered process. The initial step is exposure to LED light at 405 nm which induces polymerization in a cross sectional mode, 2-3 mm deep. The cure is then completed by adding heat at 90-95°C for 30-45 minutes. This special curing profile allows this product to be used for side bonding. Side bonding refers to when the LED light is applied between the two substrates rather than through one of them. This partial curing with the LED light from a side angle is in essence fixturing the substrates. This fast curing system is not oxygen inhibited. There are some variables to consider with speed of the LED curing process. These include the intensity of the light source, the thickness of the layer, and the width of the cross section that is being cured. The recommended intensity of the light source should be 2-4 watts/cm22.

LED422DC90 bonds well to a wide variety of substrates including plastics, glass and metals. The system has good chemical resistance to oil, water, fuels, and mild acids and bases. It is a reliable electrical insulator with a service temperature range of -80°F to 350°F. Additionally, it can withstand rigorous thermal cycling, mechanical shock and vibration. The special feature of LED422DC90 curing well cross sectionally combined with its secondary heat cure allows it to be used as a high strength adhesive. This specialty system has been used in the electronic, optical, electro-optical, and aerospace industries.

Product Advantages

  • One component system
  • Cures by LED light, UV light not required
  • Uncured material readily polymerizes with heat
  • Can cure in cross section 2-3 mm
  • Excellent strength properties, especially lap shear
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.