MasterSil 151AO

Two part silicone for high performance casting, potting & encapsulation and sealing
Key Features
  • Superior thermal conductivity
  • Low exotherm; very long pot life
  • Excellent flexibility
  • Superb electrical insulation properties
  • Can cure in thicknesses up to and beyond 1-2 inches
  • High temperatures resistance to +400°F
Typical Properties
Viscosity
Part A: 17,000-24,000 cps, Part B: 50-150 cps
Cure Schedule
48-72 hours at 75°F, 2-3 hours at 200°F
Hardness
75-85 Shore A
Service Temperature Range
-65°F to +400°F
Coefficient of Thermal Expansion
120-150 X 10⁻⁶ in/in/°C
Dielectric Strength
450 volts/mil
תמונה
MasterSil 151AO Two Part Silicone System
Certifications

MIL-STD-810G for Fungus Resistance

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond MasterSil 151AO is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151AO combines high temperature resistance, superior flexibility and very good thermal conductivity. MasterSil 151AO is an addition cured system and does not require exposure to air for complete cross-linking. It has a convenient 100 to five mix ratio by weight and will not outgas while curing. It is 100% solids and contains no solvents. MasterSil 151AO has an exceptionally low viscosity enabling it to be highly desirable for potting and encapsulation. First and foremost, MasterSil 151AO, as is true with silicones in general, offers remarkable flexibility and high temperature resistance. It has superb electrical insulation properties. Its flexibility allows it to withstand severe thermal cycling and resist vibration and shock. Also, it is very water resistant. These properties make this system well suited for applications involving sensitive optical and electrical components where heat dissipation is critical. Some additional applications include encapsulating heat generating electronic components, heat sink attachment and potting sensors, among many other uses. MasterSil 151AO is white in color. The service temperature range for this system is -65°F to +400°F.

Product Advantages

  • Addition cured; no by-products released during cure; does not require air for curing
  • Readily cures at ambient temperatures or faster cure at elevated temperatures
  • Very low shrinkage upon cure
  • Low viscosity ideal for potting and encapsulation
  • Passes fungus resistance MIL-STD-810G
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.