MasterSil 153Med

Two component, addition cured medical grade silicone for bonding and sealing
Key Features
  • Passes USP Class VI testing
  • Meets ISO 10993-5 specifications
  • Self priming feature
  • Serviceable from -65°F to +400°F
  • Paste consistency
  • Exceptionally high tensile lap shear strength
Typical Properties
Viscosity
Part A: 150,000-300,000 cps, Part B: 50,000-250,000 cps
Cure Schedule
75°F: 48-72 hours
Hardness
20-35 Shore A
Service Temperature Range
-65°F to +400°F
Dielectric Strength
450 volts/mil
Elongation
400-500%
תמונה
MasterSil 153Med Two Part Silicone
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

USP Class VI Medical

Packaging
Product Description

Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. Most significantly it can be used for medical device applications as it meets USP Class VI testing and ISO 10993-5 for cytotoxicity. MasterSil 153Med is an addition cured system and does not require exposure to air for cross-linking. It has a convenient one to one mix ratio by weight, and will not outgas while curing. It is 100% solids and contains no solvents. MasterSil 153Med exhibits typical silicone flexibility and high temperature resistance. MasterSil 153Med has an exceptionally long working life and very low exotherm. It bonds well to a wide variety of substrates including most metals, many plastics, glass and ceramic. Most importantly, it will bond well to cured silicone rubber. It has superb electrical insulation properties. Its remarkable flexibility allows it to withstand severe thermal cycling and resist vibration and shock. It has a self priming feature that enhances the bonding properties of the system. Also, it is very water resistant. MasterSil 153Med is translucent and is serviceable over the broad temperature range of -65°F to +400°F. It is widely used in medical device applications where high flexibility and splendid temperature resistance are required.

Product Advantages

  • Addition cured; no by-products released during cure; does not require air for curing
  • Low exotherm; very long pot life. Very low shrinkage upon cure
  • Readily cures at ambient temperatures or faster cure at elevated temperatures
  • Bonds well to a variety of substrates including silicone rubber. Self priming feature
  • Superior electrical insulation properties; highly resistant to water
  • Outstanding flexibility combined with high temperature resistance
  • Meets USP Class VI and ISO 10993-5 specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.