MasterSil 922-LO
One part, low outgassing silicone for bonding, sealing, coating & encapsulation
Key Features
- Meets NASA ASTM E595
- Neutral type cure
- Paste consistency
- Excellent performance profile
Typical Properties
Viscosity
paste
Cure Schedule
Recommended cure time, 75°F: 7 days
Hardness
40-50 Shore A
Service Temperature Range
-175°F to +500°F
Elongation
250-350%
Tensile Modulus
200-300 psi