Supreme 10HTND-3

One component, toughened epoxy system
Key Features
  • No mix, single component system
  • Non-drip, will not flow when applied and cured
  • Unlimited working life at room temperature
  • Wide operating temperature range
Typical Properties
Viscosity
paste
Cure Schedule
60-75 minutes at 250°F
Hardness
75-85 Shore D
Service Temperature Range
4K to +400°F
Tensile Strength
8,000-9,000 psi
Tensile Modulus
450,000-500,000 psi
תמונה
Supreme 10HTND-3 One Part Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond Supreme 10HTND-3 combines convenient handling along with high physical strength properties after curing. Most importantly this epoxy has a non-drip application feature; it will not flow when it is applied and cured. This system requires elevated temperature curing with the minimum being 250°F. Cure schedule options appear in the chart below. Since it is a true one component system, its viscosity does not change with time and the working life is unlimited.

Upon curing Supreme 10HTND-3 has extraordinarily high tensile shear and peel strength. It bonds well to a wide variety of substrates including metals, composites, ceramics, glass, and many plastics. It is a toughened system that can withstand rigorous thermal cycling along with vibration and shock. It has good chemical resistance to water, fuels, oils, as well as many acids and bases. It is a good electrical insulator after curing. Also notable is its wide service temperature range of 4K to +400°F. Its natural color is gray, but other colors are available.

Supreme 10HTND-3 blends convenient handling and exceptionally high performance properties. It is a viable candidate for the aerospace, electronic, optical, specialty OEM and related industries.

Product Advantages

  • High shear and peel strengths to a wide variety of similar and dissimilar substrates
  • Cryogenically serviceable
  • Superior thermal cycling ability
  • Unlimited working life at room temperature
  • 100% reactive; contains no solvents or diluents
  • Outstanding durability and toughness
  • Totally non flow type system
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.