Supreme 121AO

Two part toughened epoxy for bonding, sealing and encapsulation features good thermal conductivity
Key Features
  • Free flowing viscosity
  • High temperature resistance
  • Exceptionally long open time
  • Passes NASA low outgassing
Typical Properties
Viscosity
10,000-25,000 cps
Cure Schedule
1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties.
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +550°F
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F)
תמונה
Two Part Epoxy Supreme 121AO
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond Supreme 121AO is a thermally conductive epoxy for bonding, sealing and encapsulation. The mix ratio is 100:80 by weight. This system has a very long open time of 5-7 days and after mixing, it flows readily. Supreme 121AO requires oven curing. A typical cure schedule would be 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties. Supreme 121AO combines a high glass transition temperature along with an element of toughness, making it less rigid than typical higher temperature resistant epoxies.

Supreme 121AO bonds to a wide variety of substrates including metals, composites, glass, and many rubbers and plastics. It adheres especially well to glass, fibers and ceramics.

Supreme 121AO can withstand thermal cycling and mechanical stresses. Its physical strength profile is strong and steadfast, particularly its tensile modulus. It is a reliable thermal conductor while retaining excellent insulation properties. It has good resistance to chemicals including water, oils, fuels, acids and bases. The color of Part A is black and Part B is dark brown. Its service temperature range is -80°F to +550°F. It should be noted that Supreme 121AO is particularly well suited for potting and encapsulation applications. This product should be considered in demanding aerospace, electronic, optoelectronic and specialty OEM type applications where this product profile is needed.

Product Advantages

  • Good flow combined with long working life
  • Thermally conductive, electrically insulative
  • Superior physical strength properties
  • High glass transition temperature
  • Has an element of toughness
  • Combines exceptionally low shrinkage and high dimensional stability
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.