Supreme 17HTND-2

One component toughened epoxy system for bonding and sealing
Key Features
  • Convenient handling
  • Paste consistency
  • Resists thermal cycling
  • Passes NASA low outgassing
Typical Properties
Viscosity
paste
Cure Schedule
300°F for 4-6 hours or 350°F for 2-4 hours; recommended cure schedule is 4-6 hours at 300°F followed by a post cure of 8-12 hours at 350°F
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +550°F
Glass Transition Temperature (Tg)
208-210°C
Tensile Lap Shear Strength
1,900-2,100 psi at 75°F
תמונה
Supreme 17HTND-2 One Component Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond Supreme 17HTND-2 is a one component toughened epoxy for bonding and sealing. It is a paste with no flow upon curing. It is formulated to cure at 300°F in 4 to 6 hours or 350°F in 2 to 4 hours. To obtain the utmost in optimum properties, curing at 300°F for 4 to 6 hours plus a post cure of 8 to 12 hours at 350°F is recommended. It is important to note that Supreme 17HTND-2 is not premixed and frozen and its working life is unlimited at room temperature. It will only cure upon heating. The recommended storage condition for Supreme 17HTND-2 is refrigeration.

Supreme 17HTND-2 has many desirable characteristics, especially the combination of high shear and peel strength. It bonds well to a wide variety of substrates including metal, ceramics, composites and several plastics. As mentioned above, it is a toughened system, meaning that it is less rigid than a more conventional high temperature resistant epoxy. Therefore, it fits well for bonding dissimilar substrates. This toughness also imparts the capability of withstanding thermal cycling. The service temperature range is from -100°F to +550°F. It is 100% reactive and does not contain any solvents or diluents. It is a reliable electrical insulator, even at elevated temperatures. The color is black. Supreme 17HTND-2 can be considered for specialty bonding/sealing applications where convenient processing, high temperature resistance and the ability to withstand thermal cycling are important factors.

Product Advantages

  • Single component system; no mixing prior to use
  • Easy to apply
  • Good physical strength properties
  • Toughened system; fits well for bonding dissimilar substrates
  • High glass transition temperature
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.