Supreme 45HTQ-4

Two component epoxy system for bonding, sealing and casting
Key Features
  • Outstanding abrasion resistance
  • High temperature resistance
  • Can withstand high compressive loads
  • Superb chemical resistance
Typical Properties
Viscosity
paste
Cure Schedule
At 250°F, the cure time is 4-6 hours but at 300°F, this system will cure in 4-5 hours.
Hardness
85-90 Shore D
Service Temperature Range
-100°F to +450°F
Coefficient of Thermal Expansion
30-35 x 10⁻⁶ in/in/°C
Dielectric Constant
4.5
תמונה
Supreme 45HTQ Two Component Epoxy
Certifications

Meets EU Directive 2015/863

וידאו

Product Spotlight: Supreme 45HTQ-4

Supreme 45HTQ-4 is a toughened, silicon carbide filled epoxy with outstanding thermal stability and physical properties demonstrated in this video. Supreme 45HTQ-4 is very special in that it combines exceptional chemical, temperature and abrasion res …
Product Description

Master Bond Supreme 45HTQ-4 is a two component, toughened, silicon carbide filled epoxy for high performance bonding, sealing and casting. It is a specialty type system that can be used most notably in downhole applications. In fact, it can be used in a number of oil processing situations, as well as in other industrial operations. Supreme 45HTQ-4 has an easy to use 100:30 mix ratio by weight and requires oven curing at 250-350°F. (Various curing options appear in the table below.) This system’s working life is very long; 12-24 hours at room temperature. It is 100% reactive and does not contain any solvents or diluents. It has low shrinkage upon curing and is highly dimensionally stable. Supreme 45HTQ-4 is very special in that it combines exceptional chemical, temperature and abrasion resistance. It bonds well to a wide variety of substrates, including metals, composites, ceramics and many rubbers and plastics. Its service temperature range is from -100°F to +450°F and it is capable of withstanding rigorous thermal cycling. It is especially useful as a coating system. The color of both Parts A and B is gray. Supreme 45HTQ-4 can be specified in specialty type applications in oil and chemical processing, aerospace and specialty OEM when the distinctive properties mentioned previously are desirable.

Product Advantages

  • Exceptionally long pot life at room temperature
  • Robust chemical resistance
  • High temperature resistance and good strength retention
  • Stellar abrasion resistance
  • Good electrical insulator
  • Very high compressive strength
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.