UV10Med

UV curable, biocompatible, low viscosity compound
Key Features
  • USP Class VI certified
  • Fast curing
  • High bond strength
  • Electrically insulative
  • Withstands 1,000 hours 85°C/85% RH
  • Passes ISO 10993-5 for cytotoxicity
Typical Properties
Viscosity
250-500 cps
Cure Schedule
20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm²
Hardness
70-80 Shore D
Service Temperature Range
-60°F to +250°F
Refractive Index
1.557
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
UV10Med One Part UV Curable System
Applications
Certifications

1,000 Hours at 85°C/85% RH

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

USP Class VI Medical

Product Description

Master Bond UV10Med is a multi-purpose, one part UV type system for bonding, sealing and coating that features superb optical clarity and excellent physical properties as well as a very low viscosity. Most significantly it fully passes USP Class VI testing requirements. UV10Med cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and of course the intensity of the light source. It should be noted that the system can cure in sections up to 0.020-0.025 inches. However, when bonding, sections of a few thousandths of an inch are more than adequate. It bonds well to glass, surface treated metals and plastics such as polycarbonates and acrylics, among others. UV10Med is not only effective for bonding applications; it can also be used as a coating or sealant. UV10Med is resistant to many chemicals such as water, oils, bases and salts as well as sterilants including gamma, EtO and various chemical sterilants. The system does not contain any solvents or volatiles and has low shrinkage upon cure. Its service temperature range is -60°F to +250°F and it is an outstanding electrical insulator. Ideal for high production applications, particularly those involving disposable medical devices. UV10Med is also widely used in fiber-optic, optical, electronic and related industries.

Product Advantages

  • One component, no mix system
  • Exceptionally fast cure upon exposure to a UV light source at ambient temperatures
  • Low shrinkage upon cure
  • High bond strength; excellent adhesion to surface treated metals, glass and many plastics
  • Excellent optical clarity; excellent light transmission
  • Exceptionally low viscosity
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.