UV10TKMed

One component UV curable, biocompatible, high viscosity compound
Key Features
  • USP Class VI certified
  • Meets ISO 10993-5 for cytotoxicity
  • Withstands repeated sterilization
  • Superb physical properties
  • High glass transition temperature
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
35,000-85,000 cps
Cure Schedule
cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm²
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +450°F
Glass Transition Temperature (Tg)
135-140°C
Refractive Index
1.55
תמונה
UV10TKMed One Part UV Curable Compound
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

USP Class VI Medical

1,000 Hours at 85°C/85% RH

Product Description

Master Bond UV10TKMed is a higher viscosity, one part UV system for bonding, sealing and coating that passes USP Class VI testing along with ISO 10993-5 for cytotoxicity. It has exceptionally good optical clarity, sterling physical properties, a very high glass transition temperature (Tg) that exceeds 140°C and exemplary resistance to repeated sterilization. UV10TKMed cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and, of course, the intensity of the light source. It should be noted that the system can cure in sections up to ¼ inch. However, when bonding, sections of a few thousandths of an inch are more than adequate. Master Bond UV10TKMed is not oxygen inhibited and therefore does not require any special treatment in that regard. It bonds well to glass, composites, surface treated metals and plastics such as polycarbonates and acrylics, among others. It is widely used in medical devices because of its capability of withstanding repeated sterilizations, including radiation, ethylene oxide, chemical sterilants and especially autoclaving. UV10TKMed is not only effective for bonding applications; it can also be used as a coating or sealant. The system does not contain any solvents or diluents and none are released during cure. UV10TKMed combines low shrinkage with exceptional dimensional stability. Its service temperature range is -60°F to +450°F. UV10TKMed is a superlative electrical insulator. It is most effectively used in medical device manufacturing where rapid fixture times, fast curing and audacious temperature resistance are needed. UV10TKMed can be employed in a wide variety of application scenarios involving both disposable and reusable medical device manufacturing. The uniqueness of the product is based on its high temperature resistance and its ability to withstand repeated sterilizations along with a rapid UV curing mechanism.

Product Advantages

  • One component system; no mixing needed; ready to use as supplied
  • Very fine electrical insulator
  • High bond strength; excellent adhesion to surface treated metals, glass and many plastics
  • Enhanced ability to withstand repeated chemical and heat sterilizations
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.