UV15-7LRI

One part, UV curable polymer system for bonding, sealing, coating and encapsulating
Key Features
  • One component, fast curing
  • Optically clear
  • Low refractive index
  • Superior dimensional stability
  • Low viscosity
  • Rigid curing
Typical Properties
Viscosity
2,000-4,000 cps
Cure Schedule
cures quickly in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm²
Hardness
55-65 Shore D
Service Temperature Range
-60°F to +250°F
Refractive Index
1.481
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
UV15-7LRI One Part UV System
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond UV15-7LRI is a one component, low viscosity, UV curable polymer system for bonding, sealing, coating and encapsulating. The system has good physical strength properties; rigid but not brittle. UV15-7LRI cures quickly in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2. The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and of course, the intensity of the light source. It should be noted that UV15-7LRI can cure in sections from 0.080-0.0120 inches deep. However, when bonding, a section of a few thousandths of an inch is more than adequate. UV15-7LRI also possesses excellent electrical insulation properties. It is not oxygen inhibited and therefore does not require any special treatment in that regard. UV15-7LRI is optically clear with excellent light transmission properties. It bonds well to glass, surface treated metals and plastics such as polycarbonates and acrylics, among others. It is especially useful to note that the refractive index is an exceptionally low 1.481. As mentioned above, UV15-7LRI can be cured in sections with thicknesses up to ⅛ inch deep making it well suited for various electronic and opto-electronic potting and encapsulation applications. The system does not contain any solvents or volatiles and none are released during cure. UV15-7LRI offers excellent chemical resistance to water, fuels, acids and bases. Its service temperature range is -60°F to +250°F . Ideal for high production applications where fast fixture times and rapid curing are critical, UV15-7LRI is widely used in fiber-optic, optical, electronic and related industries.

Product Advantages

  • One component system; no mixing needed; ready to use as supplied
  • Exceptionally fast cure upon exposure to a UV light source at ambient temperatures
  • No air inhibition while curing; no special inert atmosphere required
  • Good electrical insulator
  • Excellent dimensional stability
  • Outstanding optical clarity; excellent light transmission
  • Low refractive index
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.