UV15-7SP4
UV system for high performance bonding, sealing, coating and encapsulation
Key Features
- Low viscosity
- Superior non-yellowing properties
- Excellent flexibility
- Low shrinkage upon cure
Typical Properties
Viscosity
800-1,500 cps
Cure Schedule
UV light 320-365 nm for 20-30 seconds
Hardness
25-30 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
3.4
Elongation
>50%
Refractive Index
1.531
Tensile Modulus
5,000-15,000 psi
Volume Resistivity
>10¹⁴ ohm-cm