UV15LV

Low viscosity, one component, UV curable epoxy based system
Key Features
  • Exceptionally low viscosity
  • Superior thermal stability
  • Very little shrinkage upon cure
  • Cationic curing system
Typical Properties
Viscosity
70-120 cps
Cure Schedule
UV light 320-365 nm for 15-30 seconds
Hardness
>75 Shore D
Service Temperature Range
-80°F to +300°F
Dielectric Constant
3.25
Refractive Index
1.517
תמונה
UV15LV One Part UV Curable Epoxy Based Compound
Certifications

Meets EU Directive 2015/863

Case Study
Case Study

UV15LV Citation

Master Bond UV15LV was used in a research article for photo-stability measurements of electropoptic polymer inverted ridge waveguides. For this application, UV curable epoxy Master Bond UV15LV1 was used to spin coat silicon wafers, to form claddings. …
Product Description

Master Bond UV15LV is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It is especially noteworthy for its low viscosity and it is widely used in a variety of applications where spin coating is required. It is also completely free of any oxygen inhibition. UV15LV will cure quickly and easily when exposed to a UV light source with a wavelength range between 320-365 nm, with the optimum at 365 nm. The energy required is typically 20-40 milliwatts per cm². The rate of cure depends upon the distance of the light from the material being cured, the thickness of the section and the intensity of the light source. It typically cures in thicknesses of a micron or less up to 0.001-0.015 inches in 15-30 seconds or less. Epoxy based UVs are described as having a “cationic” curing reaction. This kind of system will have lower shrinkage (1-2%) and higher temperature resistance than the majority of UV systems that cure by a “free radical” mechanism. UV15LV has excellent resistance to a wide variety of chemicals including water, acids, bases, fuels and many solvents. It features superb physical strength characteristics and electrical insulation properties. UV15LV has superior adhesion to a wide variety of substrates including plastics, glass and many metals. As is typical with UVs, it has excellent optical clarity and light transmission properties.

Cationic systems, such as UV15LV, tend to have much higher temperature resistance than other UV type systems. Its glass transition temperature (Tg) with a straight UV cure is about 85°C and when post cured for 30 minutes at 125°C, the Tg is about 120°C. This post cure also enhances UV15LV’s chemical resistance. The service temperature range for this system is -80°F to +300°F. It is widely used for a variety of applications in the optical, optoelectronic, aerospace and related industries.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.