UV15RCL

Red colored UV curable epoxy system turns clear upon exposure to UV light
Key Features
  • Cationic curing system
  • Not oxygen inhibited
  • Low viscosity
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
115-350 cps
Cure Schedule
UV light 320-365 nm for 30-60 seconds
Hardness
>75 Shore D
Service Temperature Range
-80°F to +350°F
Glass Transition Temperature (Tg)
90-95°C without post cure, 125-130°C with post cure
Refractive Index
1.517
תמונה
Red colored UV curable epoxy system
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond UV15RCL is a red colored, high strength, low viscosity epoxy based UV system for bonding, sealing and coating. The red color serves as an indicator as to whether UV light reaches the UV curable material. If the light reaches the material, the color will change to clear; if not, it will remain red. It is important to note that the change in color does not indicate full cure, but only that the UV light has reached the polymer.

The lamp should emit light with a wavelength range between 320-365 nm, the optimum being 365 nm. The typical energy required is 20-40 milliwatts per cm². Another variable is the distance of the light source from the material that is being cured. Taking into account these factors, full cure can generally be achieved in 30-60 seconds.

UV15RCL is a cationic curing system. It is not oxygen inhibited and will cure in sections up to 1/8 of an inch thick. UV15RCL has lower shrinkage, higher temperature resistance and good chemical resistance.

The system bonds well to a wide variety of substrates including optically clear plastics, acrylics, polycarbonates, metals, composites and many types of rubber. UV15RCL has excellent chemical resistance to water, acids, bases, fuels and many solvents. It features superb physical strength characteristics and withstands rigorous thermal cycling. As is typical with UVs, it has excellent optical clarity and light transmission properties. The service temperature range is -80°F to +350°F. It is 100% reactive and does not contain any solvents or other volatiles.

Cationic systems, such as UV15RCL, tend to have much higher temperature resistance than other UV type systems. Also, adding heat is highly beneficial to enhancing the glass transition temperature (Tg). With a curing schedule of only UV light, the Tg is about 90-95°C. However, when post cured for 1-2 hours at 125°C, the Tg increases to about 125-130°C. Post curing will also increase the product’s chemical resistance. It has wide applicability in the optical, optoelectronic, aerospace, specialty OEM, among many other high-tech industries.

Product Advantages

  • Changes color from red to clear when exposed to UV light (not an indicator of full cure)
  • Very low viscosity, spin coatable
  • Cationic cure, capable of high Tg
  • Exceptionally low shrinkage
  • Good adhesion to many substrates
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.