UV15X-5

UV system for high performance bonding, sealing, coating and encapsulation
Key Features
  • Outstanding abrasion resistance
  • Superior non-yellowing properties
  • Excellent flexibility
  • High viscosity
Typical Properties
Viscosity
175,000-235,000 cps
Cure Schedule
10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2
Hardness
30-40 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
4.5
Refractive Index
1.49
תמונה
UV15X-5 One Part UV Curable Compound
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond UV15X-5 is a one component, UV curing urethane acrylate type system featuring splendid flexibility, resounding toughness and superb abrasion resistance. This high viscosity system is multifunctional and can be used for bonding, sealing, coating and encapsulating. Possessing high elongation, UV15X-5 has the capacity to withstand severe thermal cycling and to resist thermal and mechanical shocks. UV15X-5 bonds well to a variety of substrates including glass, many plastics such as polycarbonates and acrylics, composites, metals and various rubbers. UV15X- 5 has very good chemical resistance, especially to water oils and cleaning agents. UV15X-5 is a marvelous thermal and electrical insulator with a service temperature range of -80°F to +250°F. One other favorable property is its superior non-yellowing profile.

Master Bond UV15X-5 generally cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the system’s distance from the light source, the thickness of the section and of course the intensity of the light source. It should be noted that the system can cure in sections approaching 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. Most importantly, UV15X-5 does not display oxygen inhibition. This system is widely used in fiber-optic, optical, electronic, semiconductor, microelectronic and laser applications.

Product Advantages

  • One part system with no mixing needed
  • Very fast curing upon exposure to 320-365 nm UV light at ambient temperatures
  • Impressive thermal and electrical insulator
  • Outstanding flexibility, toughness and abrasion resistance
  • Highly reliable in withstanding rigorous thermal cycling as well as thermal and mechanical shocks
  • ƒƒ
  • Wonderful non-yellowing capabilities
  • No oxygen inhibition
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.