UV22

One component, optically clear, nanosilica filled UV curable epoxy system; meets NASA low outgassing specification
Key Features
  • Exceptional abrasion resistance
  • Little shrinkage upon curing
  • Very low coefficient of thermal expansion
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
2,000-6,000 cps
Cure Schedule
UV light 320-365 nm for 15-45 seconds
Hardness
75-85 Shore D
Service Temperature Range
-80°F to +350°F
Coefficient of Thermal Expansion
30-35 ppm/°C
Refractive Index
1.52
תמונה
UV22 One Part UV Curable Epoxy
Certifications

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

ASTM D4060-14 for Abrasion Resistance

ASTM E595 Compliant

וידאו

Product Spotlight UV22

Our new video highlights the key properties of UV22, a one component, nanosilica filled UV curable epoxy system that meets NASA low outgassing specifications. This system offers exceptional abrasion resistance, superior optical clarity and thermal …
Product Description

Master Bond UV22 is a nanosilica filled, UV curable, epoxy based system for bonding, sealing, coating and encapsulation. It is 100% reactive and does not contain any solvents or diluents. There is no oxygen inhibition while curing. This nanosilica filled system is fully optically clear and has excellent dimensional stability. UV22 will cure quickly and easily when exposed to a UV light source with a wavelength range between 320-365 nm, with the optimum at 365 nm. The energy required is typically 20-40 milliwatts per cm². The rate of cure depends upon the distance from the light source, the thickness of the layer being cured and the intensity of the light source. In a relatively good set up, where the layer is thin and the light source is strong, it can cure as quickly as 10-15 seconds.

It cures in thicknesses of a few microns to about 1/8 inch in 15-45 seconds depending upon the depth of cure. UV22 has superior adhesion to a wide variety of substrates including plastics, glass and many metals. UV22 has excellent resistance to a wide variety of chemicals including water, acids, bases, fuels and many solvents. Other physical properties include enhanced abrasion resistance and outstanding dimensional stability. It is a reliable electrical insulator. As is typical with UVs, it has excellent optical clarity and light transmission properties. UV22 has exemplary low shrinkage properties, linearly less than 1%.

Epoxy based, cationic type curing systems, such as UV22, tend to have much higher temperature resistance than other UV type systems. Its glass transition temperature (Tg) with a straight UV cure is 100-110°C, and when post cured for 30-60 minutes at 125°C, the Tg is about 135-140°C. This post cure also enhances UV22’s chemical resistance. The service temperature range for this system is -80°F to +350°F. It should be noted that there’s no settling out of the nanosilica filler and the product retains its uniformity throughout its shelf life. It can be used for a wide variety of applications in the optical, opto-electronic, aerospace and related industries.

Product Advantages

  • Cationic cure, no oxygen inhibition
  • Free flowing, low viscosity
  • Enhanced dimensional stability
  • Good glass transition temperature
  • Tested for abrasion resistance per ASTM D4060-14
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.