UV22DC80-10F
One component, nanosilica filled, dual cure system with UV and heat curing mechanisms
Key Features
- Thixotropic low viscosity
- Meets NASA low outgassing specifications
- Minimal shrinkage upon curing
- Cures at 80°C in shadowed out areas
Typical Properties
Viscosity
5,000-15,000 cps
Cure Schedule
Cures at 80°C in shadowed out areas; typically the UV portion occurs in 10-30 seconds at 365 nm with 10-40 milliwatts/cm2 of output; areas not cured because of shadowing effects can be readily cured at 80°C for 30-60 minutes; post curing at 125-150°C for 15-30 minutes will increase the To significantly.
Hardness
75-85 Shore D
Service Temperature Range
-100°F to +350°F
Glass Transition Temperature (Tg)
130-135°C
Refractive Index
1.52