UV24TKLO

One component, moderate viscosity, UV curable system meets NASA low outgassing
Key Features
  • Excellent physical strength properties
  • High dimensional stability
  • Superior temperature and chemical resistance
  • Not oxygen inhibited
Typical Properties
Viscosity
40,000-55,000 cps
Cure Schedule
UV light 320-365 nm for 20-30 seconds
Hardness
80-85 Shore D
Service Temperature Range
-60°F to +400°F
Dielectric Constant
3.7
Glass Transition Temperature (Tg)
120-130°C
תמונה
UV24TKLO One Part UV Curable System
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond UV24TKLO is a one part, modified epoxy acrylate UV curable system for bonding, sealing and encapsulation. It passes the rigorous requirements for low outgassing as per ASTM E-595. It has outstanding resistance to chemicals, as described in part below. Upon curing, it should be noted that UV24TKLO is slightly translucent. The best wavelengths for curing are 320-365 nm and the energy requirement is 10-40 milliwatts per cm2. This UV system is not oxygen inhibited.

UV24TKLO has superb physical strength and electrical insulation properties. The service temperature range is -60°F to +400°F and its Tg is 120-130°C. The UV24TKLO can be cured in thicker sections, up to 1/16 of an inch and can be easily “layered” to higher levels. Most notable is that it passes the NASA low outgassing test, which enables it to be used in a wide array of applications where that property is a requirement. In order to optimize cured properties, post curing at 80-110°C for 2-4 hours is strongly recommended, if possible. Even heating at a lower temperature will enhance properties.

Product Advantages

  • One component, no mixing required
  • Not oxygen inhibited
  • Outstanding physical strength properties
  • Reliable electrical insulator
  • Relatively high Tg
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.