Case Studies

Explore real-world applications of Master Bond products and see how they solved specific challenges in various industries. These case studies offer valuable insights and inspiration for your own projects. 

 

Since 1976, Master Bond has collaborated with universities, national laboratories and other research institutions to create innovative adhesive compounds meeting their specific application requirements. As a result, Master Bond products are cited in over 300 research articles published in peer-reviewed scientific journals. They are also cited in over 800 US and international patents. Here are the most interesting cases of applications in research labs and commercial use.

Filters
Title Description Product Type Industries URI (indexed field)
EP112: Utilized to Bond Silicon Wafers to Glass Support Substrates during Microelectronics Fabrication Master Bond EP112 is an ultra-low-viscosity, electrically insulating, two-component epoxy system ideal for various applications. This two-part case study series presents two use cases for EP112 for… Two Part Epoxy Electronics, OEM /it/case-study/ep112-utilized-bond-silicon-wafers-glass-support-substrates-during-microelectronics
EP114: Utilized to produce nanocomposites via vacuum infiltration Master Bond EP114 is a two-component nano silica filled epoxy system which offers excellent dimensional stability and a very high glass transition temperature (Tg >200°C upon curing. Its ultra-… Two Part Epoxy Electrical /it/case-study/ep114-utilized-produce-nanocomposites-vacuum-infiltration
EP15: Utilized to test the bond strength of thermal spray according to ASTM C633 Master Bond EP15 is a one-component, thermally-curing epoxy with a tensile strength in excess of 12,000 psi (82.7 MPa) due to the formation of rigid, dimensionally stable bonds upon curing. This… One Part Epoxy Electrical, Materials Science /it/case-study/ep15-utilized-test-bond-strength-thermal-spray-according-astm-c633
EP15ND-2: Used in a Comparison of Tests Evaluating the Bond Strength of Thermal Sprayed Coatings Master Bond EP15ND-2 is a single component, heat curing epoxy specifically designed for testing the strength of thermal sprayed coatings as indicated by ASTM C633. Featuring exceptionally high… One Part Epoxy Materials Science /it/case-study/ep15nd-2-used-comparison-tests-evaluating-bond-strength-thermal-sprayed-coatings
Case Study EP17HTDA-1: Used in air-microfluidic particulate matter sensor for wearable devices Master Bond EP17HTDA-1 was used by researchers in an air-microfluidic particulate matter sensor for a wearable device. Exposure to airborne particulate matter can cause numerous adverse health… One Part Epoxy Electrical, Electronics, Sensors /it/case-study/ep17htda-1-used-air-microfluidic-particulate-matter-sensor-wearable-devices
EP17HTND-CCM: Electro-thermal Actuated, Miniaturized Optical Scanning Fiber Endoscope EP17HTND-CCM is a one component, heat cured epoxy system for bonding, sealing and glob top applications. This epoxy system features excellent physical properties, superb electrical insulation along… One Part Epoxy Electrical, Medical /it/case-study/ep17htnd-ccm-electro-thermal-actuated-miniaturized-optical-scanning-fiber-endoscope
Case Study EP21: Utilized in Film Sensor for Dissolved Oxygen Measurement Researchers in Germany wrote a paper on how a miniaturized sensor for dissolved oxygen was fabricated in silicon thin film technology. In this paper, they cited Master Bond as follows. “Finally, the… Two Part Epoxy Electronics /it/case-study/ep21-utilized-film-sensor-dissolved-oxygen-measurement
Case Study EP21AOLV-1 Citations Master Bond EP21AOLV-1 was used in research done by a graduate student at University of Houston. Here is a quote from this work: Two Part Epoxy Materials Science /it/case-study/ep21aolv-1-citations
EP21ARHT: Fabrication of a high-energy-resolution diced quartz spherical analyzer for RIXS Researchers at the Argonne National Laboratory document their achievement of a novel, diced spherical quartz analyzer for use in the spectroscopic method of resonant inelastic X-ray scattering (… Two Part Epoxy Materials Science /it/case-study/ep21arht-fabrication-high-energy-resolution-diced-quartz-spherical-analyzer-rixs
EP21LSCL-2Med: Encapsulating Wearable Sensors Using a Pre-Mixed Two-Part Epoxy Product This case study is a collaboration between Master Bond and Nordson. It examines the selection and implementation of a non-cytotoxic adhesive chosen for its ability to encapsulate sensors from harsh… Two Part Epoxy Medical, Sensors /it/case-study/ep21lscl-2med-encapsulating-wearable-sensors-using-pre-mixed-two-part-epoxy-product
Why Work with Master Bond

Perché scegliere Master Bond

  • Supporto tecnico personalizzato fornito da ingegneri esperti
  • Adesivi che soddisfano i più severi standard del settore
  • Prestazioni e affidabilità comprovate da centinaia di pubblicazioni su riviste scientifiche sottoposte a revisione paritaria
  • Realizzati su ordinazione per garantire la massima durata di conservazione
  • Direttamente dal nostro stabilimento di produzione negli Stati Uniti