Two part, room temperature curable epoxy adhesive, sealant, coating and casting system
Key Features
  • Convenient handling, long working life
  • High thermal conductivity and electrical insulation
  • Superior ability to withstand heat
  • Excellent chemical resistance
Typical Properties
Viscosity
Part A: 450,000-550,000 cps, Part B: 4,000-10,000 cps
Cure Schedule
cures in 3-4 days at ambient temperatures; at 200°F, the cure schedule is 2-3 hours; optimum curing is overnight at 75°F followed by 2-4 hours at 150-200°F
Hardness
85-95 Shore D
Service Temperature Range
-100°F to +400°F
Tensile Lap Shear Strength
800-1,000 psi
Tensile Modulus
600,000-700,000 psi
Immagine
EP42HT-2AN Two Component Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP42HT-2AN is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance and outstanding chemical resistance. It is widely used in a variety of potting and encapsulation applications where thermal conductivity is needed. Aside from being a superior adhesive, sealant and coating, EP42HT-2AN is castable to thicknesses exceeding 2 inches. EP42HT-2AN cures in 3-4 days at ambient temperatures. At 200°F, the cure schedule is 2-3 hours. Optimum curing is overnight at room temperature followed by 2-4 hours at 150-200°F.

EP42HT-2AN bonds well to a wide variety of substrates including metals, ceramics, composites, and many plastics. It has excellent chemical resistance to water, oils, fuels, as well as acids, bases and many solvents. The service temperature range is -100°F to +400°F. This product is a candidate for applications in electronics, electro-optics and specialty type OEM applications.

Product Advantages

  • Convenient cure schedules at both ambient and elevated temperatures
  • Excellent chemical resistance
  • Superior thermal stability
  • Outstanding thermal conductivity and electrical insulation properties
  • Good flow properties
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.