Supreme 11AO

Highlight

Two Component, Room Temperature Curing, Thermally Conductive, Electrically Isolating Epoxy For Bonding & Sealing Featuring High Shear & Peel Strength

Typical Properties
Viscosity
paste
Cure Schedule
24-36 hours at 75°F, 1-2 hours at 200°F
Dielectric Strength
>400 volts/mil
T-peel Strength
15 pli
Thermal Conductivity
10 BTU•in/(ft²•hr•°F)
Immagine
Supreme 11AO Two Component Epoxy Compound
Applications
Product Description

Master Bond Polymer System Supreme 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated temperatures with a convenient one-to-one (1:1) mix ratio by weight or volume. Its most outstanding features include high thermal conductivity, excellent electrical insulation properties, temperature resistance up to 250°F as well as superior bond strength. Supreme 11AO is a paste that can be applied without sagging or dripping even on vertical surfaces. As a toughened system, it is well suited to applications involving thermal cycling. Its chemical resistance profile includes water, oils and most organic solvents. It has excellent adhesion to most metals, ceramics, glass and vulcanized rubbers as well as many plastics. Supreme 11AO is also unique in that the bond strength is high in both shear and peel modes. Both part A and B are colored off-white. Master Bond Supreme 11AO is widely used in the electronic, electrical, computer, metalworking, appliance, automotive and chemical industries where high bond strength and superior heat transfer properties are required.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.