Supreme 3AOHT
One component, fast curing epoxy for bonding, sealing and coating
Key Features
- One part, no mix epoxy system
- Thermally conductive, eletrically insulative
- Fast curing, minimum 250°F
- Withstands rigorous thermal cycling
Typical Properties
Viscosity
Paste
Cure Schedule
250°F for 20-30 minutes; 300°F for 5-10 minutes
Hardness
>85 Shore D
Service Temperature Range
-100°F to +350°F
Coefficient of Thermal Expansion
30-35 x 10⁻⁶ in/in/°C
Dielectric Constant
4.1
Tensile Lap Shear Strength
>1,600 psi
Thermal Conductivity
9-10 BTU•in/(ft²•hr•°F) [1.30-1.44 W/(m•K)]
Volume Resistivity
>10¹⁵ ohm-cm