EP76MHT
Two component, nickel filled epoxy for bonding, sealing and coating
Key Features
- Good electrical and thermal conductivity
- Highly serviceable operating temperature
- Convenient processing
- Excellent dimensional stability
Typical Properties
Viscosity
>700,000 cps
Cure Schedule
overnight at ambient temperature followed by 3-4 hours at 150°F
Hardness
>80 Shore D
Service Temperature Range
-60°F to +400°F
Coefficient of Thermal Expansion
30-35 X 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
85-90°C
Tensile Lap Shear Strength
>2,100 psi
Thermal Conductivity
8-9 BTU•in/(ft²•hr•°F)
Volume Resistivity
5-10 ohm-cm