EP31ND
Two component epoxy system featuring exceptional bonding strength properties and paste consistency
Key Features
- Convenient handling
- Excellent structural adhesive
- Smooth paste consistency
- Provides superior electrical insulation values
Typical Properties
Viscosity
Paste
Cure Schedule
cures in about 1-2 days at ambient temperatures, 2-3 hours at 200°F; overnight cure at 75°F followed by 2-3 hours at 150-200°F is desirable
Hardness
70-80 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
4,000-4,200 psi