EP4TC-80
One component thermally conductive, electrically insulating epoxy with a curing temperature of 80°C
Key Features
- Paste consistency
- Ultra fine particle size
- High modulus and compressive strength
- NASA low outgassing
Typical Properties
Viscosity
300,000-800,000 cps
Cure Schedule
80°C for 90-120 minutes with an optional post cure of 1-2 hours at 80°C
Hardness
85-95 Shore D
Service Temperature Range
-58°F to +347°F
Glass Transition Temperature (Tg)
120-125°C
Thermal Conductivity
11-15 BTU•in/(ft²•hr•°F) [1.6-2.2 W/(m•K)]