Lab Report

Testing Adhesives for Resistance to Potassium Hydroxide (KOH)

Many Master Bond epoxy systems are formulated with superior chemical resistance. We continually test our materials by exposing them to specific chemicals over a long period of time. A common way of testing the chemical compatibility of an epoxy is immersing a sample in a chemical and measuring its change in weight over time. A significant loss or gain in weight would indicate a decreased ability of a material to stand up to chemical exposure. These tests allow us to more accurately recommend the right product based on specific application requirements.

In this experiment, we focused on testing our epoxies for their resistance to 45% potassium hydroxide (KOH). The compounds Master Bond used for testing are a variety of two component epoxies and one component UV curing systems with good overall chemical resistance. For the first round of testing, which involved exposure to 45% KOH for 10 months, the products tested were EP42HT-2AO-1 Black, EP39MAOHT, EP46HT-2AO Black, UV26, and EP41S-5LV. For the second round of testing, which involved exposure to KOH for two years, the product tested was EP42HT-2. For the third round of testing, which involved exposure to KOH for more than two and a half years, the products tested were EP62-1 (with a 100:5 mix ratio), EP41S-5, EP41S-1HT, and EP62-1HT. A few thin castings, roughly 2 inches in diameter and around 0.125 inches thick, were made for each product and cured in accordance with their specifications. Once the cured samples were created and initial weight was recorded, the castings were immersed in 45% KOH. Then, we continued recording frequent weight measurements. Below you will see the results of soaking for these various time intervals. The castings were weighed periodically, and the graphs shown below demonstrate the percentage of weight change over time.

Test results of change in weight in epoxies after exposure to 45% KOH

Test results of change in weight in epoxies after exposure to 45% KOH

Test results of change in weight in epoxies after exposure to 45% KOH

Test results of change in weight in epoxies after exposure to 45% KOH

Testing Adhesives for Resistance to KOH

For the purpose of comparison, please note that for exposures two years or longer, a casting of a standard epoxy was also tested under these same conditions which served as a reference. As can be seen in the graphs, the standard epoxy was markedly less resistant to 45% KOH than the other epoxies tested. It demonstrated a significantly greater change in weight over time and the casting ultimately dissolved in 45% KOH after approximately two years. Due to the similarity in response of the products tested for more than two and a half years, the results are shown in two separate graphs.

Chemicals can etch the surface of an epoxy (resulting in weight loss), or they can cause swelling of the sample (resulting in weight gain). In general, a weight change of less than 4-5% (gain or loss) can be considered excellent, especially since these tests may be more rigorous compared to actual service conditions. It is also worth noting that in the context of a bonded joint or a potted assembly the exposure to 45% KOH might not be as severe or direct as in the above test conditions.

Please note, when choosing an epoxy for an application where the resistance to 45% KOH is critical, many other factors must be considered in addition to the chemical resistance. Nearly all the products tested performed well, even with prolonged exposure to 45% KOH. However, depending on the time of exposure to 45% KOH, each of the epoxies in the charts above offers a distinct set of performance properties. If low shrinkage and dimensional stability are needed, EP39MAOHT can be considered. For longer term exposures, if a high glass transition temperature is needed, EP62-1HT is a good choice. EP41S-5 may be considered if electrical insulation and low outgassing are the priorities. These products all need to be processed or cured differently but the key in all cases is the addition of heat for enhancing/optimizing chemical resistance especially to 45% KOH.

Disclaimer: The findings in this article are not meant to be used for specification purposes.

Master Bond Potassium Hydroxide (KOH) Resistant Epoxies

Immagine
EP62-1HT Two Part Epoxy
Superior resistance to harsh chemicals, particularly to acids. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-160°C. Shore D hardness 80-90.
Immagine
Low viscosity, chemically resistant epoxy system EP41S-5LV
Excellent chemical resistance to solvents, alcohols, fuels, acids and bases. Low viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +350°F.
Immagine
EP39MAOHT Two Part Epoxy System
Thermally conductive, low viscosity potting/encapsulation compound. Superior dielectric properties. Versatile cure schedules. Convenient one to one mix ratio weight or volume. Minimal shrinkage and stress development. Resists thermal cycling and mechanical shocks. Service temperature range -100°F to +400°F.
Immagine
EP42HT-2AO-1 Black Two Part Epoxy
Good heat conduction. Serviceable from 4K to +400°F. Resists water, oils, fuels. Excellent dielectric properties. Enhanced dimensional stability. Castable up to 2-3 inches thick. Low shrinkage upon cure. Good flow. Meets NASA low outgassing standards.
Immagine
UV curable adhesive with high thermal stability UV26
Specialty type UV curable adhesive with very fast curing time and high thermal stability. Its glass transition temperature is 160 to 170°C and its service temperature range is -60°F to +500°F. UV26 resists acids, bases, fuels, and many aggressive solvents.
Immagine
EP41S-1HT Two Part Epoxy System
Two component, ambient temperature curing system with excellent physical properties. Thermally stable. High compressive strength. Features extraordinary resistance to fuels, alcohols and organic solvents. Withstands 1,000 hours 85°C/85% RH. Service temperature range -60°F to +400°F. Moderate viscosity. Good electrical insulator.
Immagine
EP62-1 Two Part Epoxy System
Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 120-130°C. Shore D hardness >80.
Immagine
EP41S-5 Two Part Epoxy System
Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.