Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 100-1,000 cps
Cure Schedule
60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.2 at 75°F, 60 Hz
Glass Transition Temperature (Tg)
145-155°C
Immagine
EP62-1HT Two Part Epoxy
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Product Description

Master Bond EP62-1HT is a two component epoxy system with a long working life at ambient temperature. The mix ratio is a forgiving 100 to 5 by weight. Upon mixing, it is a moderate viscosity system that flows well. The working life of 100 grams is 12-24 hours at room temperature.

There are a few cure schedule options, all requiring the addition of heat. These include 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]. To obtain optimum properties, post curing at 212-302°F [100-150°C] for 3-5 hours is recommended. Upon curing with the optimum schedule EP62-1HT displays robust temperature resistance with a glass transition temperature ranging from 150-155°C. It is highly resistant to many aggressive chemicals, most notably acids, but also many bases and solvents, even at elevated temperatures (see the chart below). EP62-1HT is a dependable electrically insulating material. The service temperature range is -60°F to +450°F. The color of Part A is clear and Part B is dark brown. A non-drip version is also available, called EP62-1HTND. It is well suited for many rigorous applications in aerospace, electronic and specialty OEM, among other industries, especially where high temperature resistance and the ability to withstand hostile chemicals is needed.

Product Advantages

  • Very long working life
  • Protects against many aggressive chemicals, even at high temperatures
  • Versatile curing schedules
  • Good flow properties
  • Low shrinkage upon curing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.