EP30LTE-4 is no longer available. We recommend EP30LTE-2 as a potential alternative. Please consult with our technical team to verify that this replacement is the most appropriate solution for your application.
Recommended Replacement Product
Immagine
Thermally conductive, electrically insulative epoxy. Has low thermal expansion coefficient. Superior dimensional stability. Good flow properties. Exceptionally low shrinkage upon cure. Service operating temperature range from -100°F to +250°F. Adheres well to similar and dissimilar substrates.