EP41S-F is no longer available. We recommend EP41S-LO as a potential alternative. Please consult with our technical team to verify that this replacement is the most appropriate solution for your application.
Recommended Replacement Product
Immagine
Certified to meet ASTM E595 for NASA low outgassing specifications. Rapid curing. Excellent chemical resistance to oils, fuels, acids, bases, solvents, chemical sterilants. Service temperature range -60°F to +250°F. Vacuum compatible. Easy to apply. High strength properties.