EP110F8-3
Two component, high performance epoxy for potting, sealing, encapsulating and casting
Key Features
- Toughened system
- Low viscosity and long working life
- Outstanding electrical insulation properties
- Very resistant to thermal cycling and shock
Typical Properties
Viscosity
1,000-2,000 cps
Cure Schedule
4-6 hours at 250-300°F
Hardness
40-50 Shore A
Service Temperature Range
-100°F to +300°F
Elongation
120-150%
Volume Resistivity
>10¹⁵ ohm-cm