EP17HT-LO

One component epoxy system for bonding, sealing, coating and casting
Key Features
  • Very high glass transition temperature
  • Meets NASA low outgassing specifications
  • Excellent compressive/tensile strength properties
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
45,000-75,000 cps
Cure Schedule
300°F for 4-6 hours, plus 12-24 hours at 350°F
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +600°F
Glass Transition Temperature (Tg)
200-210°C
Tensile Lap Shear Strength
3,000-3,200 psi at 75°F
Immagine
EP17HT-LO One Part Epoxy
Certifications

ASTM E595 Compliant

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

Product Description

Master Bond EP17HT-LO is an extraordinary one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features excellent physical properties, a superb electrical insulation profile and chemical resistance even with heat exposure to 600°F. Its glass transition temperature (Tg) is 200 to 210°C. This system is also distinctive in that it has very low exotherm upon curing and can be used in castings and encapsulations well beyond ½ inch in thickness. The minimum curing temperature for EP17HT-LO is 300°F with faster cures attainable at higher temperatures. Please refer to the curing section for additional details.

EP17HT-LO is 100% reactive and contains no solvents or diluents. EP17HT-LO bonds well to similar as well as dissimilar substrates such as metal, ceramics, plastics and composites. It resists many chemicals such as acids, bases, salts, fuels, oils and many solvents. Shrinkage upon cure is minimal. It is serviceable from -80°F to +600°F. This system is tan in color. EP17HT-LO retains its exceptional electrical insulation properties, even at higher temperatures. It should be noted, in order to obtain the optimum properties, a post cure of 2-12 hours at 350°F is recommended. As mentioned above, EP17HT-LO meets NASA low outgassing specifications. It is widely used in a variety of applications in the aerospace, oil and chemical processing, optical, optoelectronic and specialty OEM industries.

Product Advantages

  • Single component system; no mixing prior to use. Contains no solvents, diluents or volatiles
  • Easy application; only contact pressure required during heat cure
  • Superior chemical resistance
  • Exceptionally high temperature resistance
  • Low exotherm upon curing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.