EP30-3LO
Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Key Features
- Superb optical clarity
- Excellent chemical resistance
- Low viscosity and long working life
- High glass transition temperature
- Meets NASA low outgassing specifications
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
2,000-5,000 cps
Cure Schedule
1-2 hours at 170°F followed by 2-3 hours at 300°F
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +450°F
Glass Transition Temperature (Tg)
170-175°C
Volume Resistivity
>10¹⁵ ohm-cm
Immagine
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
1,000 Hours at 85°C/85% RH
Meets EU Directive 2015/863