EP37-3FLF
Two component, room temperature curing epoxy for bonding, casting and coating
Key Features
- Superb optical clarity
- Low viscosity
- Very high flexibility
- Cryogenically serviceable down to 4K
- Resists severe thermal and mechanical shocks
- Long working life and low exotherm
Typical Properties
Viscosity
600-1,200 cps
Cure Schedule
overnight at 75°F, followed by a post cure at 135-165°F for 3-5 hours
Hardness
25-35 Shore D
Service Temperature Range
4K to +250°F
Acoustical Impedance
2.5 MRayl
Refractive Index
1.536
Immagine
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
Case Study
Flexible EP37-3FLF Adhesive Excels in E-Textile Packaging Study
Master Bond EP37-3FLF was selected as one of six adhesives tested in a study of flexible electronic packaging for e-textiles conducted at the University of Southampton. For both the shear load and bending tests, Master Bond EP37-3FLF exhibited the be …