EP37-3FLSP
Two component, epoxy for high performance potting, encapsulation, sealing and bonding
Key Features
- Superb optical clarity
- Low viscosity
- Highly flexible
- Exceptionally long working life
- Low exotherm during cure
- Cures at room temperature
Typical Properties
Viscosity
300-600 cps
Cure Schedule
12-24 hours at 75°F, followed by 6-10 hours at 135-165°F
Hardness
65-75 Shore A
Service Temperature Range
4K to +200°F
Dielectric Constant
4.1
Tensile Modulus
20,000-50,000 psi