EP42HT-2Med Black
Two component, high temperature resistant epoxy for medical device assembly
Key Features
- Convenient processing
- USP Class VI approved
- Passes ISO 10993-5 for cytotoxicity
- Resists repeated sterilization, including autoclaving
Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 30-70 cps
Cure Schedule
48-72 hours at 75°F; 2-3 hours at 200°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.0 at 75°F, 60Hz
Glass Transition Temperature (Tg)
150-155°C
Immagine
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ISO 10993-5 for Cytotoxicity
Meets EU Directive 2015/863
USP Class VI Medical