EP46HT-1AO
Two part, thermally conductive, electrically insulative epoxy for bonding and sealing featuring outstanding heat resistance; requires oven curing
Key Features
- Impressive thermal conductivity and electrical insulation
- High glass transition temperature
- Excellent physical properties & dimensional stability
- Meets MIL-STD-883J Section 3.5.2 for thermal stability
- Meets NASA low outgassing specifications
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Paste
Cure Schedule
2 hours at 300°F, followed by a few hours at 350-400°F
Hardness
85-95 Shore D
Service Temperature Range
-100°F to +550°F
Dielectric Strength
450 volts/mil
Tensile Modulus
550,000-650,000 psi