EP46HT-1ND-2
Two component epoxy paste for structural bonding featuring superlative heat resistance; requires oven curing. Will not flow during processing
Key Features
- Glass transition temperature over 240°C
- Impressive chemical resistance
- Outstanding electrical insulation properties
- Long pot life at room temperature
- Service temperature range of -100°F to +600°F
- High bonding strength
Typical Properties
Viscosity
paste
Cure Schedule
250-300°F for 2-3 hours, followed by a post cure for optimum properties at 350-400°F for 2 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +600°F
Dielectric Strength
450 volts/mil
Tensile Lap Shear Strength
>2,200 psi