Supreme 11AOHT-LO
Toughened, high strength, two component epoxy for bonding and sealing
Key Features
- Convenient handling
- Thermally conductive & electrically insulative
- Withstands 1,000 hours 85°C/85% RH
- NASA low outgassing approved
Typical Properties
Viscosity
Part A: 200,000-300,000 cps, Part B: paste
Cure Schedule
overnight at 75°F followed by a few hours at 150-200°F
Hardness
80-90 Shore D
Service Temperature Range
-112°F to +400°F
Coefficient of Thermal Expansion
35-40 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
3,200-3,400 psi
Immagine
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Certifications
1,000 Hours at 85°C/85% RH
Meets EU Directive 2015/863
ASTM E595 Compliant
Packaging
Video
Thermally Conductive, NASA Low Outgassing Epoxy System Supreme 11AOHT-LO
Master Bond Supreme 11AOHT-LO is a two component epoxy resin system for high performance bonding and sealing.
Its most outstanding features include high thermal conductivity, excellent electrical insulation properties and temperature resistance up t …